Alpha Alumina Low Viscosity Polishing Slurry, 0.05 micron, ALPHA-NANO-1005

$27.00
Shipping calculated at checkout.

0.05 µm Alpha Alumina Low Viscosity Polishing Slurry is available in 16 oz, 32 oz, 1/2 gallon, and 1 gallon.

Volume: 6 oz
Abrasive Size: 0.05 µm
Shipping & Returns

Upon delivery, the customer must inspect the products within ten (10) business days. Report any issues to pace@metallographic.com within thirty (30) business days of delivery, including the invoice number and relevant details. Failure to report within this period means acceptance of the products.


Returns are subject to a 15% restocking fee unless the products are non-conforming, in which case the fee is waived after inspection. Returned products must be in original condition. PACE Technologies may amend the restocking fee for specific products or orders.

Volume: 6 oz
Abrasive Size: 0.05 µm