Epoxy (Glass-Reinforced) Compression Mounting Resin

Epoxy (glass reinforced) is a compression mounting resin used in metallographic sample preparation. This material provides excellent adhesion, chemical resistance, and enhanced mechanical strength due to the glass reinforcement. It produces a clear, hard mount that is ideal for protecting and preserving delicate or porous specimens during grinding, polishing, and examination.