SiC Grinding

Comparison of standard US grit size to European grit and micron size

Standard grit 120 180 240 320 360 400 600 800 1200
European
(P-grade)
P120 P180 P280 P400 P500 P600 P1200 P1500 P2500
Abrasive particle
size (microns)
125 82 52 35 30 26 15 13 8
Filter and sort 193 products
Sort by

Metallographic Equipment

Pace Technologies provides a comprehensive range of metallography equipment, including cutting, mounting, grinding, and polishing solutions to meet all your material analysis needs.