SiC Grinding
Explore our comprehensive Silicon Carbide (SiC) grinding solutions, including SiC Papers, Foils, Rolls, and Powders, for precise and efficient metallographic surface preparation. Available in various grit sizes, these products ensure optimal results at different stages of sample preparation.
Comparison of standard US grit size to European grit and micron size
Standard grit | 120 | 180 | 240 | 320 | 360 | 400 | 600 | 800 | 1200 |
European (P-grade) |
P120 | P180 | P220 | P320 | P500 | P800 | P1200 | P2400 | P4000 |
Abrasive particle size (microns) |
106 | 75 | 58.5 | 40.5 | 30.2 | 21.8 | 15.3 | 6.5 | 2.5 |